Printing with TPU requires a different approach than standard hard plastics. TPU, or thermoplastic polyurethane, is a flexible material. The most common hardness encountered is 95A on the Shore scale. It is highly resistant to abrasion and impacts. This article summarizes how to print TPU correctly.
What TPU 95A is used for
Thanks to its flexibility and durability, TPU has a wide range of uses. It is not just for toys. We print phone cases from it ourselves, which absorb drops perfectly. Furthermore, it is perfectly suited for various vibration dampers under machines, custom seals or tires for RC models. It is also frequently used for flexible hinges on boxes, where standard plastic would break after a few bends. If a part needs to bend or resist mechanical wear, TPU filament is the clear choice.
Extruder: Direct drive versus Bowden
The type of extruder makes a fundamental difference when printing TPU. A direct drive extruder, where the feeding gear is located directly above the nozzle, is strongly preferred for flexible materials. The filament path is very short and the strand has no room to bend or escape to the side.
Printing on a printer with a Bowden setup is possible but requires great patience. The strand is soft and flexes in the long PTFE tube. With a Bowden setup, printing must be slow, typically at a speed of 20 to 40 mm/s. Retractions must be minimal for both types of extruders, or it is better to turn them off completely. Every time the soft strand is pulled back, the risk of jamming increases.
Feeding issues and how to avoid them
The most common issue when printing TPU is the filament wrapping around the feeding gear. This occurs when the resistance in the nozzle is greater than the strength of the strand. The strand then bends and escapes through the gap in the extruder. The solution is simple. Print slowly. Increase the nozzle temperature so the material flows better. Ensure the extruder is assembled correctly and that there is no unnecessarily large gap between the feeding gear and the hotend entrance.
Drying is absolutely essential
TPU is a highly hygroscopic material. This means it absorbs moisture from the air very quickly. Wet filament pops during printing, forms bubbles and strings extremely. Before printing, dry it at 50 to 55 °C for 4 to 8 hours. Use a filament dryer or a food dehydrator. An oven is risky due to temperature fluctuations, and the spool can deform. After drying, store the strand in a sealed box with silica gel. For more details, read the article on drying filament.
Bed adhesion and removing prints
While with other materials the struggle is getting the print to stick to the bed, with TPU the problem is the opposite. TPU sticks too well to a smooth PEI sheet. If printed directly on a clean sheet, there is a risk of tearing off the bed surface during removal. Always use a thin layer of glue stick as a separator. The glue ensures the print can be safely removed after cooling. The bed does not need to be heated extremely; 0 to 60 °C is sufficient.
Recommended print settings
Here is an overview of proven settings for TPU. These can be used, for example, for our black TPU Prof. Lab.
| Parameter | Value |
|---|---|
| Nozzle temperature | 210 to 230 °C |
| Bed temperature | 0 to 60 °C |
| Print speed (Bowden) | 20 to 40 mm/s |
| Retraction | Minimal or off |
| Drying | 50 to 55 °C for 4 to 8 h |
Frequently asked questions (FAQ)
Why does material ooze from the nozzle even during travel moves?
This is caused by pressure in the nozzle and disabled or small retractions. With flexible materials, this cannot be completely avoided. It helps to dry the material thoroughly and enable the avoid crossing perimeters function in the slicer so that any strings remain inside the model.
Can TPU be sanded or otherwise surface treated?
Sanding TPU is very difficult. The material yields and pills. It is best to print it directly so that the surface is satisfactory. Any strings can be carefully cut off with a sharp scalpel.
How to tell if TPU is wet?
During extrusion, quiet popping or hissing will be heard. Tiny bubbles will appear on the surface of the print and the material will string much more. A wet spool will also result in poorer layer strength.
Is an enclosed printer necessary for TPU?
No. TPU does not need an enclosed chamber. It is not prone to warping due to drafts like ABS or ASA. It prints without issues on open printers.
Can TPU be printed on a printer with AMS or another automatic feeder?
Most automatic feeders cannot handle soft TPU. The strand jams in the long tubes and mechanisms. We recommend always loading TPU manually directly into the extruder via an external spool holder.